Specifications:
- Sensor type: Ceramic sensor plate
- Temperature range: Cryostat cooling: –50 ºC till 700 ºC
- Temperature accuracy: ±0.2 ºC
- Thermocouples: 56 (FRS5) or 120 (HSS7) thermocouples
- Digital resolution: 16 million points
- Resolution: 0.04 µW
- Number of sample positions: 34